| Proof Stress (RP0.2) | 600 MPa |
| Ultimate Tensile Strength | 770-780 MPa |
| Tensile Elongation | >3% |
| Elastic Modulus | 200-230 GPa |
| Vicker Hardness | (Hv30) 330-380 |
| Density | 8.3 - 8.4/cm3 |
| Thermal Expansion Coefficient | 13.4gm/m.°C (25 500°C) |
| Melting Range | 1400-1430°C |
| Solidification Range(cooling) | 1285-1350°C |
| Cr | 29% |
| Mo | 5,9% |
| C | Max. 0,50% |
| Co | Balance |
| Fi | Max. 0,7% |
| Si | Max. 1% |
| Other | Max. 0,5% |
•Cr :29%
•Mo :5,9%
•C :Max 0,50%
•Co :Balance
•Fe :Max. 0,7%
•Si :Max. 1%
•Other:Max.0,5%